I actually rolled and brushed the material around the pond. The stuff is quite thick, and based on their specific recommendation I did not thin the material. I cannot imagine using a sprayer, as the cleaning would be a nightmare.

In my opinion, grinding down dry material and adding water to mix it up does not constitute "OEM" manufacturing status. The raw material is developed by someone else. This reminds of my last trip to the health food store, where I actually saw “Oxygenated Water” – based on your assumption the person that packaged that farce must have also been the “Original Manufacturer” of Oxygen + Water!!